Yes, you can put Legos in resin, but you need to weigh the bricks down, pour in stages, and wait for a full cure. According to Apex Resin’s Lego tutorial, most deep pour resins are mixed 2:1, while general purpose resin is mixed 1:1, and the mix should run at least three minutes. Its Deep Cast resin can be poured up to 30cm in one pour and was left 48 hours before unmolding. Plaid’s Lego frame project says to allow 24 hours for the resin to harden before sanding.
Clear casting resin can hold Lego bricks well, and the process is more forgiving than it looks. The main challenges are bricks that float or tip, air trapped inside hollow studs, and plastic that may react with the wrong product. This guide walks through what happens inside the pour, how to pick a resin, and how to work through bubbles and cure times without guessing.
What Happens When You Put Legos in Resin
Lego bricks are not all the same weight once they are sitting in liquid resin, so their behavior varies. Some bricks float up, some tip onto their sides, and some stay put. Apex Resin notes that pieces often float or tip during a pour, and tweezers can help you reposition them.
Lego bricks are made mostly of ABS plastic. According to the Lego timeline on Wikipedia, the company moved away from cellulose acetate to the more stable ABS in 1963. That detail matters because your resin needs to bond to and cure around a plastic that is not porous like wood. Expect the bond to be mechanical more than chemical, so the bricks stay put mainly because they are held inside the cured block.
Hollow bottoms and open studs can trap air. Apex Resin’s Lego tutorial recommends pouring resin into the bricks first, which helps weigh them down and reduces the number of air pockets that release bubbles later. Plan your layout before you mix, because the first layer decides where most bricks will sit.

Choosing the Right Resin and Preparing the Bricks
The right resin depends on how deep your pour is and whether you need one layer or several. Deep pour casting resins and general purpose resins use different mix ratios, so reading the bottle matters. Use the table below as a starting point, then follow the manufacturer’s instructions for your exact product.

| Resin type | Mix ratio named in sources | Best use with Legos |
|---|---|---|
| Deep pour casting resin | Usually 2:1 (Apex Resin) | Solid blocks, letters, and thick molds with bricks fully covered |
| General purpose resin | 1:1 (Apex Resin) | Thin layers, such as a picture frame base coat |
| Mod Podge Resin style kits | Follow the package for mixing (Plaid) | Shallow frame projects with bricks set in a first layer |
Before you pour, clean every brick and remove dust, since debris can cloud the finish. Basecoating a wooden frame first, as Plaid’s project does with a paint, also helps you judge color contrast under the clear layer. Let the paint dry fully before you tape or pour.
Check the resin’s technical data sheet and safety data sheet for plastic compatibility and UV stability. Some resins are rated for use outdoors or in sunlight, and that rating matters if your piece will sit near a window. If the sheet is unclear, test the resin on a spare brick and watch it for a few days before you commit a finished piece.
Step-by-Step Process for Embedding Legos in Epoxy
The core method is the same across the sources: mix carefully, set the bricks in a first layer, then pour the rest in stages. Stepping through each phase in order keeps bricks from drifting and keeps bubbles from building up in one pour.
- Mix the resin fully. Measure each part in its own cup, then combine and stir for at least three minutes, scraping the sides. Apex Resin warns that poor mixing can leave the resin flexible or unset.
- Pour a base layer. Plaid’s frame project pours a thin layer of clear resin first, then arranges the Legos on top.
- Set the bricks. Press each brick into the wet layer. Mod Podge Rocks brushes a little resin on the bottom of each brick before it goes down.
- Wait for the first layer to grab. Mod Podge Rocks lets the bricks set for 20 minutes, with about 30 minutes of working time in the cup.
- Pour the rest slowly. Pour around the bricks rather than onto them, and adjust any that tip with tweezers.
- Release bubbles gently. Apex Resin suggests waiting 10 minutes after each pour, then passing a crafting heat gun lightly over the surface.
- Let the piece cure. Leave it undisturbed for the full time on the label. Apex Resin’s deep pour sat 48 hours before unmolding.
Tip: Mix in a larger cup than you think you need, then pour into a second cup before you start. Scraping the bottom of the first cup helps you catch unmixed resin.
For a deeper look at how other objects are suspended inside a casting, the guide on rocks in resin covers similar weight and layering issues.
Preventing Bubbles, Yellowing, and Cracks
Bubbles are the most common complaint, and the fix is usually slower mixing and controlled heat. Mixing slowly, as Apex Resin describes, reduces the bubbles you introduce in the first place. Hollow bricks still need attention, so release any trapped air before the resin begins to set.
Heat is useful, but it can cause harm when overdone. Happi Crafts warns against over-torching resin because it will ruin the finish, and Apex Resin says to keep the heat moving so you do not overheat the resin or damage the mold. Short, light passes are the safer habit.
Yellowing and clouding usually come from the resin itself, from moisture, or from light exposure over time. Choose a resin whose data sheet describes UV stability if the piece will sit in sun. Keep the mixing area dry, and cover curing pieces to keep dust out, since Apex Resin uses covers for this purpose.
Cracks and edge shrinkage are normal signs that the resin is still curing. Apex Resin notes that even good resin shrinks slightly, which can leave a small edge on the piece. Lightly sand that edge with fine sandpaper, such as 2000 grit, once the piece has fully cured.
Curing Time, Temperature, and Safety Tips
Curing time depends on the resin and the depth of the pour, so follow the label first. The sources in this guide used 24 hours before sanding for a shallow frame and 48 hours before unmolding a deep pour. Do not rush the process, because a partly cured piece can dent, tack, or pick up marks.
Temperature affects cure speed, and the package will list a recommended working range. Keep the room steady, away from drafts and direct heat sources, while the piece sets. If you are unsure whether your space is suitable, check the resin’s data sheet rather than guessing.
Wear nitrile gloves and work in a ventilated space. Plaid’s Lego frame project lists a respirator among the supplies, so check the safety data sheet for your product and follow its recommended protection. Keep resin off your skin, and clean tools before the resin cures.
Safety: Read the safety data sheet for your resin before you start. Use gloves, good ventilation and a respirator if the sheet calls for one.
If you are planning a larger collection of embedded items, the overview on Inclusions & Embedding explains how layering choices affect what you see in the finished piece.
Troubleshooting Common Lego Resin Problems
Most Lego resin problems come from mixing, timing or bricks that were not prepared well. Match the symptom to the likely cause below, and change one variable at a time so you can see what helped.
| Symptom | Likely cause | What to do |
|---|---|---|
| Resin stays soft or tacky | Incomplete mixing or wrong ratio (Apex Resin) | Remeasure, mix at least three minutes, and allow the full cure time |
| Bricks float or tip | Pouring over bricks without a base layer | Pour into the bricks first and reposition with tweezers |
| Many small bubbles | Fast stirring or an overworked torch or heat gun | Stir slowly and use short, light heat passes |
| Edges look uneven | Normal shrinkage during cure (Apex Resin) | Sand lightly with fine grit after full cure |
Bubbles that appear after the resin has set are usually trapped air that rose slowly. If the surface is still tacky, a light pass of heat may help, but avoid overworking the spot. Persistent cloudiness is worth checking against the data sheet for moisture or temperature limits.
For a Lego picture frame, a second pour over the sides is common. Plaid’s project wraps the back in tape, then pours the resin again so it runs over the edges. Remove the tape only after the resin has set.
Frequently Asked Questions
Can you put Lego bricks in epoxy resin?
Yes. Many makers embed Lego bricks in epoxy by pouring a first layer, setting the bricks, then pouring the rest. Apex Resin recommends pouring resin into the bricks first to weigh them down and reduce floating.
Do I need a silicone mold to make resin Legos?
No. Mod Podge Rocks describes two methods, one using only a silicone mold and one using a wood frame with tape and poured resin. Happi Crafts uses a silicone mold to make resin Lego-style pieces that can be stacked for play.
How long does resin take to harden before sanding?
Plaid’s Lego frame project allows 24 hours before rounding edges with sandpaper. Apex Resin’s deep pour was cured 48 hours before unmolding. Always follow the label for your product, since cure times vary between brands.
Will resin melt or damage Lego bricks?
The sources do not describe resin melting Lego bricks, and Lego bricks are made of ABS plastic. Check your resin’s data sheet for compatibility with plastics, and test a spare brick before you embed a finished piece.
Once you know the basics, you can apply them to frames, coasters, or small molded projects. Start with a shallow test pour, keep your brick colors in mind, and write down your mix ratios and cure times so the next piece goes faster.
More in Inclusions & Embedding
How to Mix Glitter into Resin Without Clumping or SinkingUpdated Nov 26, 2026
Resin Projects with Dried Flowers: How to Prep, Seal and Cure Them RightUpdated Nov 26, 2026
Hair in Resin: Why It Floats, Bubbles or Yellows, and How to Prevent ItUpdated Nov 26, 2026
Can You Put Fresh Flowers in Resin? Why They Brown and How to Dry Them RightUpdated Nov 26, 2026
Wood in Resin: Which Woods Work and How to Seal Them for Clear, Bubble-Free ResultsUpdated Nov 26, 2026
How to Preserve Dried Flowers in Resin So They Stay Bright and FlatUpdated Nov 26, 2026