How to Make a River Table with Epoxy, Step by Step
Posts by Laura WhitfieldNovember 26, 20260 Comments
8 min read · by Laura Whitfield · Updated
We may earn a commission when you buy through links on this page, at no extra cost to you. Learn more.
Learning how to make a river table means joining two live edge slabs, building a sealed mold around them, and pouring epoxy into the gap between them. Sources recommend wood with a moisture content of 6% to 10%, and they advise avoiding wood at 12% or higher. Epoxy cure times range from 24 hours to several days depending on the product and thickness. A typical build also includes sanding up to 400 grit and a finish before the table is ready to use.
This guide walks you through the full process for a first river table. You will read what the build involves, which materials and tools matter, how to prepare the wood and mold, how to pour and remove bubbles, and how to cure, level and finish the top. If you are learning how to make a river table for the first time, the steps below are in the order most builders follow.
What Is a River Table and How It Works
A river table is a tabletop made from two live edge slabs with a gap filled by a pourable material, usually clear or tinted epoxy resin. The natural edges of the slabs act as the riverbanks, and the resin becomes the water running between them. According to Flowyline, live edge slabs are the standard starting point, and walnut and olive are common choices.
Each table is unique because the wood edges are unique. The gap width, the color of the resin and the shape of the river are all design decisions you make before you buy supplies. Lancaster Live Edge notes that a wider river will need more epoxy, so plan the gap early.

Materials and Tools You Need
Gather everything before you mix any resin, because a pour that stalls halfway can leave a visible line. The list below covers the core items that sources mention for a basic build. Check the technical data sheet for your specific epoxy to confirm the mix ratio and maximum pour depth.
| Item | What it is used for |
|---|---|
| Live edge hardwood slabs | Form the banks of the river; should be kiln-dried |
| Moisture meter | Checks wood moisture in several spots before you start |
| Circular saw or track saw, with straight edge | Rips the slab along a straight centerline |
| Jointer and thickness planer, or slab flattener | Makes the faces flat so resin does not seep under the wood |
| Melamine or MDF panels, or HDPE sheet | Builds the mold; melamine and HDPE resist sticking |
| Silicone caulk and sealant tape | Seals seams and inside corners against leaks |
| Clamps, screws and weights | Stop the slabs from floating in the resin |
| Deep pour epoxy with mixing containers and stir sticks | Fills the river; read the maximum pour depth on the label |
| Heat gun | Releases surface bubbles during the first hour |
| Sandpaper from 120 to 400 grit, and an orbital sander | Prepares the wood and smooths the cured resin |
| Gloves, goggles and a respirator | Protects skin, eyes and lungs during mixing and sanding |
Tip: Buy a little more epoxy than your math says. Lancaster Live Edge suggests adding about 10% for loss and overflow, and a short pour is much harder to fix than a spare cup.
Prepare the Slab and Build the Mold
Start with dry wood, because moisture trapped in the slab can cause bubbles and soft spots in the cured resin. Lancaster Live Edge recommends kiln-dried hardwood at 6% to 10% moisture content and advises avoiding slabs at 12% or higher. Check several spots with a moisture meter, and reject slabs with soft rot or large end cracks.
Next, rip the slab along the centerline with a straight edge and a circular saw, making several shallow passes. Then flatten each half. FixThisBuildThat ran its halves through a jointer and then a planer, and it noted that the planer must be wide enough to handle the finished width. Lancaster Live Edge describes flattening with a slab flattener or router sled in passes 2 to 3 millimeters deep, then sanding the top to 120 grit so the epoxy has something to grip.
Before you build the mold, clean the wood. Remove loose bark with a chisel or brass brush, vacuum the dust, and wipe the surface with isopropyl alcohol. Lancaster Live Edge says water can raise the grain, so alcohol is the safer wipe. Seal the end grain with a thin coat of epoxy, which helps prevent air from escaping into the main pour.

Build the mold from 3/4 inch MDF, melamine or an HDPE floor, according to FixThisBuildThat and Lancaster Live Edge. FixThisBuildThat sealed the mold’s inside corners with sealant tape and wrote that silicone would have been faster for the three-way corners. Melamine is a common choice because, according to The Accent Piece, neither epoxy nor concrete sticks to it, though a release agent is still recommended for epoxy.
Make the mold just wide enough for the slabs, and set the slabs upside down if your tabletop surface is the bottom face. Lancaster Live Edge recommends a thin bead of caulk along the mold ends and under each slab, then clamping the slabs down flat so they form a small dam against leaks. For a deeper study of mold options, see how to make an epoxy river table, which covers the same build with more detail on the forms.
Mix, Pour and Remove Bubbles
Calculate your volume before you mix. Multiply the river’s length by its width and depth in inches, divide the result by 231 to get gallons, and add about 10% extra. Lancaster Live Edge gives an example of a river 48 inches long, 2 inches wide and 1 inch deep, which comes to 96 cubic inches. Measure the resin and hardener by the ratio on the label, since an incorrect ratio can leave the resin soft or bubbly.
Follow these steps once the mold is sealed and the slabs are clamped:
- Warm the resin. Lancaster Live Edge suggests bringing it to about 70 to 80 degrees Fahrenheit.
- Mix slowly. Stir for about five minutes and scrape the sides and bottom of the container.
- Add color if you want it. Use mica or liquid dye within the limits on the label.
- Check the pour depth. FixThisBuildThat used a 2 to 1 epoxy that could be poured up to 1-3/4 inches at a time, and UltraClear’s deep pour product is formulated for up to 2 inches. Pour in layers if your river is deeper than the label allows.
- Pour slowly down the center. Let the resin flow under the edges on its own.
- Run a heat gun over the surface. Lancaster Live Edge recommends doing this every 10 to 15 minutes during the first hour. Keep the gun moving so the resin does not scorch.
- Cover the mold. Lay a light plastic sheet over it to keep dust out while the resin sets.
Bubbles come from trapped air, so mixing slowly and sealing the wood help more than any single fix. Flowyline notes that a heat gun can pop surface bubbles, and UltraClear says a seal coat makes bubble removal much easier. Check the surface again after the first hour, because some bubbles rise later.
Safety: Wear gloves and goggles while mixing, work in a ventilated room, and read the safety data sheet for your epoxy. Keep a respirator on hand for sanding dust.
Cure, Level and Finish the Table
Do not rush the cure. Flowyline says epoxy can take anywhere from 24 hours to several days, depending on the type and the thickness. FixThisBuildThat’s build cured for 72 hours before the slab was released. Follow the cure time on your product’s label, and keep the room at a steady temperature.
After demolding, remove the clamps and screws and wedge the slab off the base with shims. FixThisBuildThat found that epoxy leaked under the slabs and dropped the surface below the wood, so it planed the top level. Lancaster Live Edge notes that a waxy film called amine blush can form on the cured surface. Wash it off with warm soapy water and dry the table before sanding.
Sand from coarse to fine. Lancaster Live Edge describes a wide belt sander at 220 grit, then an orbital sander at 320 and 400 grit until the scratch pattern is even. FixThisBuildThat sanded the wood to 180 grit and the epoxy to 400 grit. Finish with a clear epoxy, oil or polyurethane, and let it cure fully before you attach legs. For a source with the moisture guidance in full, read the Lancaster Live Edge river table guide, which lists the moisture ranges and sanding grits used in this article.
Frequently Asked Questions
How long does river table epoxy take to cure?
Flowyline gives a range of 24 hours to several days, depending on the epoxy type and the thickness. FixThisBuildThat’s build cured for 72 hours. Check your product’s label, because the manufacturer’s time is the one to follow.
How thick can I pour river table epoxy in one go?
It depends on the product. FixThisBuildThat’s 2 to 1 epoxy could be poured up to 1-3/4 inches at a time, and UltraClear’s deep pour epoxy is formulated for up to 2 inches. Pour in layers if your river is deeper than the label allows.
What moisture content should live edge wood be for a river table?
Lancaster Live Edge recommends kiln-dried hardwood at 6% to 10% moisture content. It advises avoiding wood at 12% or higher. Check several spots with a moisture meter before you commit to a slab.
What safety gear do I need when working with river table epoxy?
Sources recommend gloves, goggles and a respirator, especially during sanding. Read the safety data sheet for your product and work in a ventilated space. Wash off any amine blush with warm soapy water as part of cleanup.
Take your time with the wood and the mold, because most river table problems start there. Once the slabs are flat and sealed, the pour is the easy part. If you want to compare design options next, see epoxy river table ideas, or browse the Wood, Tables & Countertops section for more builds.
More in Wood, Tables & Countertops
How to Epoxy Live Edge Wood: A Step-by-Step Guide to a Flat, Durable TabletopUpdated Nov 26, 2026
How to Fill Knots with Epoxy for a Smooth, Durable Wood SurfaceUpdated Nov 26, 2026
Outdoor Bar Top Epoxy: How to Pick a UV-Resistant Resin and Cure It RightUpdated Nov 26, 2026
How to Make an Epoxy River Table: Step-by-Step Build for BeginnersUpdated Nov 26, 2026
Pine Epoxy Table Guide: How to Prep Softwood for a Clean River PourUpdated Nov 26, 2026
Spalted Maple Epoxy Table: How to Stabilize, Pour, and Care for OneUpdated Nov 26, 2026