You can put wood in resin, and dense hardwoods like maple, walnut, cherry and cedar usually give the best results. Wood in resin works when the wood is dry, sanded and sealed before the main pour. According to Resiners, keeping the room steady at about 70–75°F while the epoxy cures helps the result stay clear. Most wood projects also need a full cure of 24 to 72 hours, depending on the product you choose.
This guide walks you through the practical side of embedding wood in epoxy. You will see which woods tend to work, how to prepare and seal them, how to manage bubbles, and what usually goes wrong when a piece comes out cloudy or cracked.
Can You Put Wood in Resin?
Yes, wood can be embedded in epoxy for a sealed, glossy piece. The main challenge is that wood is porous and holds air, so the preparation matters more than the pour itself.
Woodworking Advisor’s epoxy prep guide describes the seal coat as the step most guides skip, and it is the difference between a bubble-free finish and a frustrating one. Wood also changes size slightly with temperature and humidity, so the epoxy you choose should be one made for wood projects.
Before you start, check the product’s pour depth. Table top formulas are generally meant for pours up to about a quarter inch, while deep-pour formulas can fill an inch or more in one layer, according to the same source.

Which Woods Work Best for Resin Embedding?
Dense hardwoods are the easiest starting point for most makers. Maple, walnut, cherry and cedar are listed as solid choices that bond well with resin and sand down nicely.
Softwoods tend to soak up too much resin, so they are harder to control. Open-grain and porous woods such as pine and fir need a seal coat before the main pour, because trapped air in those pores is what causes bubbles.
Oily woods like teak and rosewood need one extra step. Wipe the surface with acetone or naphtha just before applying epoxy, and test on a scrap first, since some finishes react differently. For a wider view of the same system, see How to Fill Holes in Wood with Epoxy.
| Wood type | How it behaves in epoxy | What to do |
|---|---|---|
| Maple, walnut, cherry, cedar | Bonds well and sands cleanly | Sand, clean and check for dryness |
| Oak, pine, fir (porous) | Absorbs resin and traps air | Apply a thin seal coat first |
| Teak, rosewood (oily) | Oils interfere with adhesion | Wipe with acetone or naphtha, then test |
| Softwoods in general | Soak up too much resin | Use with care and expect extra resin use |
Tip: Open-grain woods can use up a lot of resin, so buy a little extra before you start a large piece.
Preparing and Sealing Wood Before Pouring
Preparation decides most outcomes. Sanding, cleaning and sealing all happen before you mix any resin for the main pour.
Resinpro recommends sanding from 80 grit through 120, 240 and 320. Woodworking Advisor suggests a progression of 80–120, then 150–180, then 220–320 for the final pass. Vacuum and wipe with a tack cloth afterward, because any dust left behind gets trapped in the finish.
Next, brush on a seal coat. This is a thin layer of the epoxy itself, not a separate sealer. Let it sit until it is tacky, commonly around 4 hours depending on the product and room temperature, then pour the flood coat while the seal is still slightly sticky so the layers bond.

Safety: Wear nitrile gloves rather than latex and keep the wood dry and free of dust before you mix. Check the product’s SDS for ventilation guidance.
Pouring Techniques to Avoid Bubbles
Bubbles come from air escaping the wood, from mixing too fast and from pouring too thick in one go. Careful mixing and pour depth control solve most of them.
Mix the resin and hardener at the ratio on the label, commonly 1:1 or 2:1. Stir slowly for a couple of minutes while scraping the sides and bottom, because fast stirring pulls more air into the mix.
Pour steadily rather than all at once. Wait 5 to 10 minutes for bubbles to rise, then pass a heat gun or torch 6 to 8 inches above the surface, moving quickly. Resinpro also advises coating the underside and base of forms with a catalyzed resin layer of at least 2–3 mm so air cannot hide under the wood. A related explanation is in How to Make Wood and Resin Coasters.
Curing Times and Temperature Considerations
Cure time and temperature control how clear and hard the finished piece becomes. Rushing either one usually shows up as a soft or cloudy surface.
Resiners wood and resin guide recommends a steady temperature of about 70–75°F during cure. Full cure can take 24 to 72 hours depending on the resin, while some manufacturers list 72 hours to more than 7 days before final sanding and heavy use. Read your product’s data sheet for its exact numbers.
Thick pours create heat. Most casting resins are limited to layers of no more than about 2 cm, and overly thick layers can overheat, cure unevenly and trap bubbles. Keep the piece level and dust-free the whole time.
Tip: Wood that is not dry enough can cause cloudiness, so check moisture before you seal. Wood should sit around 7–12% moisture content, measured with a meter if you have one.
Common Problems and How to Fix Them
Most failures trace back to damp wood, poor cleaning, under-mixed resin or too much depth in one pour. Identifying the symptom helps you fix the right cause.
| Symptom | Likely cause | Fix |
|---|---|---|
| Bubbles that keep appearing | Porous wood without a seal coat | Seal first, then pop bubbles while still liquid |
| Epoxy pulling away from edges | Oils or contaminants on the wood | Clean, sand lightly and reapply |
| Cloudy or soft patches | Damp wood, wrong ratio or cold room | Dry the wood, measure carefully and keep the room warm |
| Surface yellowing over time | Standard epoxy exposed to sun | Use a UV-resistant epoxy and a UV-protective topcoat |
Cracks often come from pouring too deep at once or from heat building up during cure. Choose a product rated for your pour depth, and split very thick pieces into layers. The manufacturer’s data sheet lists the maximum depth for each product. Readers working through this often move on to Epoxy on Pallet Wood.
Safety Tips When Working With Wood and Epoxy
Epoxy resin and hardener are skin and eye irritants, and repeated skin contact can lead to allergic sensitization that builds with each exposure. Good habits protect you every time you work.
Wear nitrile gloves and safety glasses, and work in a ventilated space. Some epoxies release vapors while curing, so consider a respirator if the product’s SDS recommends one. Wash any skin contact right away with soap and water.
Safety: Read the product’s SDS before you start, and keep uncured resin away from children and pets.
Frequently Asked Questions
What kind of wood works best for resin projects?
Dense hardwoods such as maple, walnut and cherry are listed as strong choices because they bond well and sand smoothly. Cedar is also mentioned as a solid option. Softwoods tend to soak up too much resin.
Do you need to seal wood before pouring epoxy over it?
For porous wood, yes. A thin seal coat lets trapped air escape before the flood coat goes on. Let the seal coat become tacky, commonly around 4 hours, before pouring the thicker layer.
How do you get rid of bubbles when pouring resin on wood?
Mix slowly, scraping the sides and bottom, and wait 5 to 10 minutes for bubbles to rise. Then pass a heat gun or torch 6 to 8 inches from the surface, moving quickly. Work while the epoxy is still liquid.
How long does epoxy take to cure on wood?
Full cure often takes 24 to 72 hours with some resins, and some manufacturers list 72 hours to more than 7 days. Keep the room at a steady temperature near 70–75°F and check your product’s data sheet for the exact time.
Once you know which woods suit your project and how to seal them, you can plan your first pour with confidence. For more background, read our guide on rocks in resin or explore Inclusions & Embedding to compare other materials you can set inside clear epoxy.
More in Inclusions & Embedding
How to Mix Glitter into Resin Without Clumping or SinkingUpdated Nov 26, 2026
Resin Projects with Dried Flowers: How to Prep, Seal and Cure Them RightUpdated Nov 26, 2026
Hair in Resin: Why It Floats, Bubbles or Yellows, and How to Prevent ItUpdated Nov 26, 2026
Can You Put Fresh Flowers in Resin? Why They Brown and How to Dry Them RightUpdated Nov 26, 2026
How to Preserve Dried Flowers in Resin So They Stay Bright and FlatUpdated Nov 26, 2026
How to Make Cells in Resin with Silicone Oil, Heat and Pigment ControlUpdated Nov 26, 2026