Bubbles in Resin: Causes, Prevention and Step-by-Step Fixes
Posts by Emily SawyerNovember 26, 20260 Comments
7 min read · by Emily Sawyer · Updated
We may earn a commission when you buy through links on this page, at no extra cost to you. Learn more.
Bubbles in resin form when air gets trapped during mixing, pouring, or when it rises out of porous surfaces like wood. Most of them can be removed while the resin is still wet. ACP Composites advises folding hardener into resin rather than whipping it, and says a single layer should generally be no thicker than 1/8 inch. Solid Solutions recommends working between 20°C and 30°C and warming cold sealed bottles in lukewarm water for 10 to 15 minutes before mixing.
If you have poured a clear coat or river table and found tiny bubbles across the surface, the cause is usually predictable. This guide explains where the air comes from, how to stop it before it forms, and how to handle bubbles while the resin is wet or after it has cured.
Why Bubbles Form in Epoxy and Resin
Most bubbles happen because air gets into the mix or into the project before the resin has time to release it. Knowing the source tells you which fix to use. Mixing, porous surfaces, thick pours and cold resin are the four causes that come up most often.
Air Whipped In During Mixing
Aggressive stirring pulls air into the resin, and those tiny bubbles can stay suspended as the material cures. Power mixing at high speed or in a small batch has the same effect. Terrazzo-USA advises mixing for 2 to 5 minutes while scraping the sides and bottom several times.
Air Released From Porous Surfaces
Wood, paper and woven fabric contain pockets of air. When resin flows over them, that air expands and rises through the coating. ACP Composites notes that timber outgasses most when its temperature is rising, so warm sunlight or a nearby heater can make the problem worse.
Pours That Are Too Thick or Too Cold
A deep pour can trap air below the surface before it escapes. Cold resin is thicker and holds bubbles longer. Solid Solutions describes cold resin as syrupy, which is a sign that the bottles need warming before you mix.

| What you see | Likely cause | First step |
|---|---|---|
| Tiny bubbles throughout the mix | Air whipped in while mixing | Mix slower and scrape the sides |
| Bubbles rising from wood or fabric | Outgassing from porous material | Seal the surface first |
| Bubbles that stay in a thick pour | Pour too deep for one layer | Pour in thinner layers |
| Thick, sluggish resin with bubbles | Resin is cold | Warm the sealed bottles before mixing |
How to Prevent Bubbles in Resin
Prevention is far easier than repair, so the bulk of your results depend on how you mix, seal and pour. Each step below removes a source of air before it reaches the surface. Work through them in order on every project.
Mix carefully and avoid whipping. ACP Composites guidance on preventing air bubbles explains that folding hardener into resin introduces far less air than fast whipping. Primaloc advises against using a power drill for batches under one gallon, keeping the drill on medium speed, and starting it only once the mixing bit is submerged.
Seal porous surfaces before the main coat. Primaloc recommends a thin seal coat of epoxy on porous substrates, which fills the pores so air can escape before the flood coat. Wood should be sealed, and any stain should be checked for compatibility with the resin.
Pour in controlled layers. ACP Composites says a single layer should generally be no thicker than 1/8 inch, and that you should wait until the first layer is firm and about as tacky as masking tape before adding the next. For encapsulation, pouring from the bottom of a container produces the fewest bubbles, according to the same source.

Tip: Warm sealed bottles in lukewarm water below 95°F to lower viscosity, as Terrazzo-USA suggests, and let mixed resin sit briefly before you pour.
How to Get Rid of Bubbles in Epoxy While It Is Wet
Bubbles are easiest to remove while the resin is still liquid. Heat, a fine alcohol mist or a pin can bring them to the surface where they pop. Choose the gentlest method that works for the size of the bubble.
For small bubbles, hold a low-intensity heat source above them and let the warm air draw the bubbles up. Solid Solutions says a heat gun should be held about 5 cm above the surface and moved quickly. A torch should be held several inches away and never allowed to touch the resin.
If you prefer not to use a torch, you can breathe gently through a straw over the bubbles. Denatured alcohol misted lightly over the surface can also pop bubbles, but test it on a small area first because it can blush the resin. For larger bubbles, push a pin into the bubble and wobble it so the air reaches the surface.
How to Remove Bubbles from Epoxy with a Heat Gun
A heat gun is one of the most common tools for clearing a wet flood coat. The key is short, steady passes rather than long pauses in one spot. Used this way, the warmth thins the surface and lets trapped air escape.
Follow these steps on a freshly poured surface:
- Check the timing. Work while the resin is still wet and within the early part of its cure, shortly after pouring.
- Hold the gun about 5 cm above the surface. Solid Solutions gives this distance for a heat gun.
- Sweep across the bubbles. Move left to right in one smooth pass rather than hovering.
- Limit time in one spot. Primaloc says not to linger more than 1 second, since longer heat can cause damage.
- Inspect and repeat. Look for missed or new bubbles and make another pass if needed.
For more detail on tool settings and distances, see this heat gun for resin bubbles guide. Heat should never be applied directly to a flammable epoxy surface, and you should check the product SDS before using any flame.
Safety: Wear nitrile gloves, work with good ventilation, and read the product SDS before using any heat source near resin.
How to Fix Bubbles in Epoxy After Curing
Once resin has hardened, heat cannot bring bubbles back to the surface. The fix is mechanical: sand the surface, clean it, and recoat. The method depends on whether the bubbles sit near the surface or deep in the finish.
For bubbles at or near the surface, Primaloc’s cured bubble removal steps begin with light sanding, then an acetone wipe followed by 30 minutes for evaporation. Next, apply a fresh seal coat and wait 4 to 6 hours for it to partially cure. Finish with a new flood coat over the whole surface.
Solid Solutions recommends sanding flat at 800 grit or finer before polishing and applying a thin fresh flood coat. Deeper bubbles require heavier sanding to reach them, and Primaloc advises recoating the entire surface rather than spot-treating, since spot work can leave an uneven finish.
Micro Bubbles and Common Mistakes That Cause Bubbles
Micro bubbles are very small and often appear when resin is stirred too fast or poured cold. They can be harder to see until the surface cures, so careful prevention matters. Many of the common mistakes below are easy to avoid once you know them.
Learn more about the tiny bubbles that stay suspended in a finish in this guide to micro bubbles in resin. Terrazzo-USA notes that vacuum chambers can degas resin before deep pours, which helps when surface torching is not practical.
- Whipping the hardener into the resin instead of folding it in.
- Skipping the seal coat on wood or other porous material.
- Applying resin while wood is warming in sunlight or near a heater.
- Using a foam roller that has not absorbed resin first.
- Working in a humid room, where Terrazzo-USA advises keeping relative humidity below 60%.
Frequently Asked Questions
What causes air bubbles in epoxy resin?
Bubbles usually come from air whipped in during mixing, air released from porous surfaces like wood, pours that are too thick, or resin that is too cold to let air rise. Each cause has a different fix, so identify the source first.
How do I get bubbles out of resin without a torch?
You can breathe gently through a straw over the bubbles while the resin is wet. Denatured alcohol misted lightly can also pop them, but test it first because it may blush the resin.
Is a heat gun safe for removing bubbles from epoxy?
A heat gun can be used on wet resin when you keep it moving and hold it about 5 cm from the surface. Avoid lingering in one spot, and check the product SDS and your ventilation before you start.
How do I fix bubbles in epoxy after it has cured?
Heat cannot remove cured bubbles, so sand the surface flat, usually at 800 grit or finer. Then clean it, apply a thin seal coat if needed, and add a fresh flood coat once the seal is partly cured.
Bubbles are usually preventable with slow mixing, sealed surfaces and thin pours. For other defects, visit the Troubleshooting & Fixes section. Start with the cause you suspect, then test your method on a small area before you work the full piece.
More in Troubleshooting & Fixes
How to Fix Scratches in Epoxy Tables Without Redoing the Whole TopUpdated Nov 26, 2026
How to Remove Amine Blush From Epoxy Without Starting OverUpdated Nov 26, 2026
What Will Remove Epoxy from Wood, Metal, Skin and Hair SafelyUpdated Nov 26, 2026
Paint and Epoxy Remover: Which Type Strips Cured Epoxy and Paint SafelyUpdated Nov 26, 2026
Why Is My Epoxy Bumpy? Causes and Fixes for a Smooth FinishUpdated Nov 26, 2026