Learning how to fill cracks in wood with epoxy comes down to two steps: stabilize the crack with thin penetrating epoxy, then fill the gap with a thicker epoxy filler. TotalBoat’s penetrating epoxy sealer mixes at a 2:1 ratio by volume and has a 20-minute working time at 80°F. Its FixWood putty mixes at a 1A:1B ratio and has a 30-35 minute working time at 72°F. Plan on days, not hours, for a full cure before heavy sanding.
This walkthrough shows you how to pick the right epoxy for a crack, prepare the wood, mix and pour, tint the repair, and avoid the bubbles and sinking that ruin many first attempts. The steps apply to tables, boats, and furniture, though the exact products and temperatures you use should come from the manufacturer’s data sheet for your project.
What Kind of Epoxy Works for Wood Cracks
Two broad types of epoxy handle wood cracks, and they do different jobs. A thin penetrating sealer soaks into dry, porous, or soft fibers. A thicker putty or filler bridges the gap and holds its shape while it cures.

Most cracks benefit from both. The sealer strengthens the surrounding wood, and the filler gives you the body to fill the void. TotalBoat’s guide says the two can be combined, and many makers do it that way. TotalBoat’s penetrating epoxy sealer page describes the product as a low-viscosity sealer that penetrates wood fibers.
| Product type | Best for | Key numbers from the manufacturer |
|---|---|---|
| Penetrating epoxy sealer | Hairline cracks, bare or porous wood, soft fibers | 2:1 by volume; maximum pour depth less than 1/16 inch |
| Epoxy putty and wood filler (FixWood) | Gaps, voids, and missing sections that need shaping | 1A:1B; working time 30-35 minutes at 72°F; sandable in less than 6 hours at 72°F |
| Clear epoxy resin or deep pour resin | Larger, clear-filled cracks in a finished piece | Check the product’s max pour depth before you pour |
For a river table or deep pour, a penetrating sealer is the wrong tool because TotalBoat rates its maximum pour depth at less than 1/16 inch. Use a casting resin rated for the depth you need, and check the label before you pour.
Tools and Materials You Need
Gather everything before you mix. Epoxy has a limited working time, and stopping to look for a stir stick can mean a cured cup in your hand. A short list of basic supplies covers most crack repairs.
Set up a clean, ventilated work area with the piece supported level. Keep the repair area dry and at a temperature the product allows.
- Penetrating epoxy sealer and, if the crack is wide, a filler such as FixWood putty
- Mixing cups and stir sticks, plus a flexible spreader or putty knife
- Syringes or a small brush for getting sealer into fine cracks
- Painter’s tape and wax paper or a release film to protect nearby wood
- Nitrile or latex gloves, and eye protection
- A heat gun for releasing trapped bubbles, used with care
- A scraper or chisel for removing loose or rotted fibers
- Tints such as alcohol inks, mica powders, or pigment dispersions, if you plan to color the repair
- Sandpaper or a sanding block, and a respirator if you sand a putty product
Prepare and Clean the Crack
Preparation decides how well the epoxy bonds. Dust, oil, and moisture block penetration, so the wood needs to be clean and dry before any product goes in. Take time here, because it is the step most often skipped.

Work from the outside of the crack inward. Remove anything that will not stay bonded, then make sure what remains is solid wood.
- Clean the crack. Remove dust, debris, and loose fibers with a brush or compressed air. Wipe away oils and grease with an appropriate solvent, and let the wood dry completely.
- Check moisture. Confirm the wood is dry before you apply any epoxy. Epoxy will not bond well to damp fibers.
- Remove rot. If the wood is soft or crumbling, use a scraper or chisel to take out the weak material until you reach firm wood.
- Protect the surroundings. Tape off areas you do not want epoxy on, and cover the back side of the crack if epoxy might run through.
Check the existing finish too. TotalBoat says its penetrating epoxy should go onto bare, unfinished wood, and it may not level well over some stains. Test an inconspicuous spot first, and do not apply it over Minwax oil-based stains, according to the manufacturer.
Seal, Mix, and Pour the Epoxy
Sealing comes before filling. A thin penetrating coat saturates the wood fibers and gives the filler a stable base to grip. Mix each product exactly as its label says, because a wrong ratio is the most common cause of a sticky or soft repair.
Use the ratio the product lists, and measure by volume or weight as the data sheet allows. Mix only what you can use within the working time.
- Warm the bottles if needed. TotalBoat’s guide recommends standing sealed resin and hardener bottles in warm water to lower viscosity, which helps reduce bubbles.
- Mix the penetrating sealer. Combine 2 parts resin A with 1 part hardener B by volume, and stir slowly to avoid whipping in air.
- Apply the sealer. Brush or syringe it into the crack until the wood stops absorbing it. On porous woods, TotalBoat advises a thin seal coat first to help prevent bubbles and curing issues.
- Wait for the right moment. If the wood is soft from dry rot, TotalBoat says to apply FixWood while the penetrating epoxy is still tacky.
- Mix the filler. Knead equal amounts of FixWood part A and part B until the mix is a light tan color with no streaks.
- Press it in. Push the putty firmly into the crack to force out air pockets. Overfill slightly so you have material to sand flush later.
- Release bubbles. Pass a heat gun briefly over the surface to bring trapped bubbles up, keeping the gun moving so you do not scorch the wood.
Tint and Match the Color
Color has to go into the epoxy before it cures. TotalBoat’s guide says cured epoxy cannot be stained, so you cannot wipe a color on afterward and expect it to soak in.
Add tints to the mixed epoxy in small amounts, using alcohol inks, mica powders, or pigment dispersions. Test the color on a scrap piece of the same wood, and let it cure before you judge the match. Putty products can be stained or painted to match surrounding wood, according to the FixWood product description, so the filler can be colored on the surface after the cure. If this section raised more questions, How to Fill Knots with Epoxy may answer them.
Curing Time and Sanding Smooth
Curing time depends on the product and the temperature. Cold slows the cure, and the penetrating sealer is sold in separate regular and cold weather formulas for that reason. Read the label for your product, then wait the full time before sanding.
The published numbers below are from TotalBoat’s data for each product. Treat them as starting points, and adjust for the room you are working in.
| Product | Temperature | Working or pot life | Full cure |
|---|---|---|---|
| Penetrating epoxy, regular | 80°F | 20 minutes | 2 days |
| Penetrating epoxy, cold weather | 40°F | 40 minutes | 4 days |
| FixWood putty | 72°F | 30-35 minutes working time | 5-7 days; sandable in less than 6 hours |
Sand only after the product reaches the stage the label describes. The FixWood product page lists sandable time as less than 6 hours at 72°F, while the full cure takes 5 to 7 days. Sanding early can gum up the surface, so wait for the full time when the repair will carry load.
Start with a medium grit to bring the overfill down flush, then move to finer grits. Keep the sanding block flat so you do not dip the repair. Once sanded, you can topcoat with paint, stain, or varnish, following the product’s topcoat guidance.
Common Problems and Fixes
Most crack repair problems come from three causes: the wrong temperature, a poor mix, or trapped air. Each one has a practical fix. Identify the symptom first, then adjust your next attempt.
If bubbles keep rising, slow down the pour and release them with a heat gun. If the surface sinks after curing, the filler probably needed more overfill to begin with.
- Bubbles: warm the bottles, mix slowly, seal porous wood first, and use the heat gun briefly to bring them up.
- Sinking or dips: overfill the crack slightly, then sand back to flush. A thick filler holds its shape better than thin sealer, which is why the two products are used together.
- Soft or sticky spots: check the mix ratio and the temperature. Penetrating epoxy should not be used as a fast-cure product in warm conditions, according to TotalBoat’s warning.
- Color that does not match: add tint before the epoxy cures and test on scrap wood. Cured epoxy cannot be stained.
- Gap too wide for a thin sealer: thicken the epoxy with colloidal silica to a peanut butter consistency, which TotalBoat’s blog describes for gap fillers.
Tip: Keep a small test batch of mixed epoxy in a cup. If it stays soft after the expected cure time, the mix ratio or temperature is the likely cause.
Safety: Wear nitrile or latex gloves and eye protection when mixing and kneading. When sanding FixWood, TotalBoat advises gloves, protective clothing, face protection, and a proper respirator. Read the product’s Safety Data Sheet before you start.
Frequently Asked Questions
Can I fill wood cracks with epoxy resin for a river table or deep pour?
Penetrating sealer is not meant for deep pours, since TotalBoat rates its maximum pour depth at less than 1/16 inch. Deep pour and table top resins have their own depth limits, and some are rated for only small castings. Check the data sheet before you pour a thick layer.
Does epoxy wood filler shrink after curing?
TotalBoat describes FixWood as a non-shrinking putty that holds its shape while it cures. That said, overfill slightly so you can sand the repair flush once it is fully cured. Shrinkage claims come from the manufacturer, so compare them with the product you buy.
Do I need to seal wood before applying epoxy filler?
For soft, porous, or dry rotted wood, sealing first helps. TotalBoat says penetrating epoxy can consolidate soft wood, and the filler should go on while that sealer is still tacky. On porous woods, a thin seal coat also helps prevent bubbles.
What temperature is needed to apply epoxy to wood?
The regular penetrating sealer is labeled for 65 to 90°F, and the cold weather formula for 40 to 65°F. FixWood can be applied from 50 to 100°F. Use the formula that matches your shop temperature, and keep the workpiece at that range while it cures.
A clean, well-sealed crack lasts much longer than a quick patch. For more background, see what is marine epoxy, and browse Boats, Repairs & Bonding for related repair projects. If you are planning a larger surface, the table top epoxy instructions cover pour depth and leveling.
More in Boats, Repairs & Bonding
TotalBoat Tabletop Epoxy Cure Time: When to Sand, Recoat and Use ItUpdated Nov 26, 2026
TotalBoat Tabletop Epoxy Instructions: Mix, Pour and Cure Your Table RightUpdated Nov 26, 2026
How to Fix Epoxy Countertop Ripples, Cracks and Dull Spots Without Starting OverUpdated Nov 26, 2026
What Is Marine Epoxy? Uses, Types and Boat Repair BasicsUpdated Nov 26, 2026