How to Pour Epoxy Resin in Molds Without Bubbles or Sticking
Posts by Amanda PierceNovember 26, 20260 Comments
9 min read · by Amanda Pierce · Updated
We may earn a commission when you buy through links on this page, at no extra cost to you. Learn more.
Here is how to pour epoxy resin in molds: measure the ratio exactly, mix for the full time on the label, and pour a thin stream into one spot from 1–2 inches above the mold. Most epoxies work best between 70°F and 80°F, and colder rooms make the resin thick and more likely to hold bubbles. Pour deep molds in stages rather than all at once, since table top epoxy is rated up to 1/4 inch per layer while some casting resins go up to 2 inches per layer. Wait for the cure time on the data sheet before you demold.
Learning how to pour epoxy resin in molds takes more than a steady hand, since most failed castings trace back to the setup, the mixing, or using a resin that is not rated for the depth. This walkthrough covers what to gather, how to choose a mold material, how to prep and seal it, and how to handle bubbles and demolding. Ratios and times differ by brand, so check the manufacturer’s data sheet for your exact product.
What You Need Before You Pour Epoxy Resin
Gather your resin, mixing tools, mold, and protection before you open any containers. Some casting resins have a working time of only a few minutes, so setup has to be finished first.
Start with a level surface. Resin self-levels, so even a slight tilt sends it to the low side while it cures. Place a small bubble level on the mold itself, not just on the table, and shim it with folded paper or cardboard until the bubble sits centered. Keep your room in the working range the product lists, and warm the space if it is cold before you mix.
| Item | Why you need it |
|---|---|
| Casting resin matched to the mold depth | Deep-pour resins are rated for 1 to 2 inches per layer, while table top epoxy is rated up to 1/4 inch |
| Two clean mixing cups | The two-cup method helps keep unmixed resin out of the pour |
| Stir sticks, and a helix mixer for large batches | Lets you scrape the sides and bottom evenly |
| Bubble level and folded paper or cardboard shims | Confirms the mold sits level so the resin spreads evenly |
| Heat gun or butane torch | Pops surface bubbles; a torch is used only on open surfaces, never silicone |
| Silicone mat or plastic sheeting | Protects the table from drips that can bond permanently |
| Nitrile gloves, eye protection, and ventilation | Protects your skin, eyes, and airways while you handle resin |
Keep a lint-free cloth nearby for wiping the mold. Dust and lint left in a silicone mold will show up in the finished casting, so check the cavity once more before you mix.
Choosing the Right Mold Material for Epoxy
Silicone and melamine with tuck tape are the two most common mold choices for epoxy. The wrong material can bond to cured resin and make release nearly impossible.
Silicone molds are self-releasing, so they need no release agent. A light mist of mold release spray is optional and can extend the mold’s service life. Check for tears or holes before each pour, because liquid resin will find them. For a deeper look at release options, read do you need mold release for silicone molds.
Melamine-coated MDF with tuck tape is the usual choice for large, flat pours such as river tables. Tuck tape covers seams, corners, and raw edges where resin could leak. According to the Superclear guide to epoxy molds, melamine does not bond to epoxy, so the piece releases cleanly when the seams are sealed. Avoid raw wood, cardboard, and most foam, which can bond to resin or distort from heat. Browse the Molds & Mold Making category to compare options for your project size.

Step-by-Step: Mixing and Pouring Epoxy Resin
Follow these steps in order, because each one prevents a common failure. The biggest source of soft spots is a mistake in the ratio or in the mixing.
Many table top and art epoxies use a 1:1 ratio by volume, while some marine or structural epoxies use 2:1 or 3:1. Resin and hardener have different densities, so a volume ratio does not match a weight ratio. Confirm which measurement the product uses before you pour anything.
- Confirm the ratio and depth rating. Check whether the product is 1:1, 2:1, or another ratio by volume, and confirm the depth it is rated for.
- Prep and seal the mold. Clean and dry the mold, tuck-tape melamine seams, and seal any raw wood with a thin seal coat.
- Measure precisely. For a volume-based 1:1 system, fill both parts to the same line before mixing.
- Mix for the full time. TotalBoat’s two-cup method calls for mixing the first cup for 3–5 minutes while scraping the sides and bottom.
- Transfer to a clean cup. Pour into a second cup and mix for another 2–3 minutes, scraping again, so any unmixed resin on the first cup stays behind.
- Pour a thin stream. Hold the cup 1–2 inches (3–5 cm) above the mold and pour into one spot, letting the resin spread on its own.
- Pour in stages if the mold is deep. For depths deeper than about 1/4 inch, pour in layers and let each one reach the tacky stage before the next.
- Level and leave it alone. Recheck the bubble level, and do not move the mold once the resin starts to gel.
Do not scrape the bottom of the mixing cup into the mold. The film clinging to the walls can contain unmixed resin that creates sticky patches. Pour slightly less than you think you need, then top up, since resin that runs over the mold edge is hard to remove.
Tip: For large batches, the UltraClear pouring guidance suggests a batch of about 1 gallon when using a drill, with the mixing bit kept in the lower half of the batch at medium speed to limit air.
Removing Bubbles from Poured Resin
Most bubbles come from mixing and pouring rather than from the resin itself. A few that reach the surface can be removed with gentle heat within the first minutes after the pour.
Wait about two minutes after pouring before you reach for a heat tool, because bubbles need time to rise. Pass a heat gun 6–8 inches above the surface in slow sweeps. A torch belongs at 4–6 inches above an open surface such as a tray, and it should never be used on a silicone mold. Do not linger on one spot, because scorched resin can wrinkle or yellow. Mixing technique is the main defense against air, and the few bubbles that remain can usually be removed with a heat gun or propane torch.
Look for bubbles at a low angle by crouching so you face the light across the surface. Stubborn bubbles against an embed or a mold wall may need a gentle poke with a toothpick. Check again at 10 and 20 minutes, because new bubbles can keep rising for the first half hour.

Safety: Wear nitrile gloves, eye protection, and work with good ventilation. Read the product’s safety data sheet before you start. Keep isopropyl alcohol away from any open flame, since alcohol is flammable.
Curing Time and Demolding Your Casting
Cure time depends on the product, so the data sheet sets your demold schedule. Do not pull a casting out before the listed time, even if the surface feels firm.
Working time is the window you have before the resin begins to gel. For UltraClear Table Top Epoxy the working time is 5 minutes, while UltraClear Deep Pour Epoxy gives you 20 to 30 minutes depending on batch size. Liquid Glass Deep Pour, as described in the Superclear mold guide, has a 10–12 hour gel time and can be demolded at 48–72 hours.
| Product example | Working or gel time | Demold time | Full cure |
|---|---|---|---|
| UltraClear Table Top Epoxy | 5-minute working time | Check the product sheet | Check the product sheet |
| UltraClear Deep Pour Epoxy | 20 to 30 minutes, depending on batch size | Check the product sheet | Check the product sheet |
| Liquid Glass Deep Pour 2:1 | 10–12 hour gel time | 48–72 hours | 30 days |
| 24 Hour Liquid Glass 2:1 | Check the product sheet | 24–36 hours | 30 days |
Full cure is not the same as demolding. Liquid Glass is firm enough to handle at 48–72 hours but does not reach maximum hardness until 30 days. Handle the piece gently during this period, and avoid stacking or stressing edges. For deep pours, stay toward the lower end of the product’s temperature window, since larger volumes generate more heat as they cure.
Common Pouring Mistakes and How to Fix Them
Most pour problems come from resin depth, mixing, or mold prep. Matching the symptom to the cause makes the fix much faster.
| Symptom | Likely cause | How to fix it |
|---|---|---|
| Sticky or soft spots | Unmixed resin from the cup walls or a ratio error | Measure to the line, scrape the sides and bottom, and use a second cup |
| Bubbles throughout the middle | Fast pour or a drill bit raised too high | Pour a thin stream and keep the mixing bit in the lower half of the batch |
| Cloudy or cracked casting | One pour deeper than the product rating, or too much heat | Pour in stages and keep the room within the listed temperature range |
| Resin leaking from the mold | Open seams or corners in a melamine mold | Tuck-tape every joint and check for gaps before mixing |
| Casting bonded to the mold | Raw wood, cardboard, or an unsealed surface | Use silicone or sealed melamine, and seal any wood first |
| Thin layer that won’t cure properly | Table top epoxy used in a deep mold | Switch to a deep-pour casting resin matched to the depth |
Cold rooms cause thick resin that traps air, while overly hot conditions can set the resin too quickly or cause cracking. Warm the workspace before mixing if the room is cold, and keep the mix at a steady temperature. If a layer has already fully cured, lightly sand the surface before adding the next layer so it bonds properly.
Frequently Asked Questions
How thick can you pour epoxy resin in one layer?
It depends on the product. The UltraClear guide lists its table top epoxy at 1/8 inch per layer and most other table top epoxies at 1/16 inch. Its deep pour epoxy goes up to 2 inches per layer, with 1 inch recommended, and most other casting resins go up to 1 inch.
What mold release do I need for epoxy resin molds?
Silicone molds usually need no release agent, though a light mist of release spray is optional. Some plastics and other surfaces need release if you do not want the epoxy to bond. Test an unfamiliar plastic with a small drop of resin in a corner first.
Can you use table top epoxy for deep molds?
Table top epoxy should not replace deep-pour casting resin. Superclear’s guide notes that Table Top 1:1 is rated up to 1/4 inch and is designed for coatings. Pouring it deep can cause heat buildup, cracking, or a failed cure.
Do I need to seal wood before pouring epoxy into a mold?
Yes, porous wood should get a thin seal coat before the main pour. The seal coat helps lock in air that would otherwise rise as bubbles and dry spots. If the seal coat cures fully before you pour, lightly sand it with 220 to 320 grit and wipe it with 90% or higher isopropyl alcohol.
Once your casting is out, clean and dry the mold so it lasts for the next pour. Proper storage helps silicone stay flexible, so read how to store silicone molds before you put your molds away.
More in Molds & Mold Making
What Kind of Resin for Molds Gives You Clean, Detailed CastsUpdated Nov 26, 2026
How to Make Resin Molds for Beginners: Materials, Steps and FixesUpdated Nov 26, 2026
How to Make Resin Bowl Molds at Home, Step by StepUpdated Nov 26, 2026
Can You Use Resin Molds for Candles? What Holds Up to Hot WaxUpdated Nov 26, 2026
How to Make Resin Keychains with Molds, Step by Step for BeginnersUpdated Nov 26, 2026