Dimples in epoxy are small pits or divots that form on the cured surface, usually from trapped air bubbles, dust, contamination, or a temperature swing during cure. Most shallow dimples can be fixed with a fresh flood coat, while deeper ones need sanding and filling. According to ArtResin, you should keep the room stable at 75-85°F (24-30°C) during the first 24 hours of cure. Manufacturers also commonly note that a doming resin self-levels to about one-eighth of an inch.
Dimples look alarming, but the cause is usually traceable once you know what to check. This guide matches each type of surface defect to its likely cause, then walks through the fix. It also covers prevention so the next pour stays smooth.
What Dimples in Epoxy Look Like
Dimples are the small round holes, pits, and low spots that appear on the surface after a pour. Some people call them fish eyes, though the terms overlap in practice. Resin Obsession notes that its readers often use the two words for the same defect.
The size and shape matter for diagnosis. Tiny pinholes usually point to bubbles. Round craters with a raised edge often point to contamination. Wavy, orange-peel texture usually points to a coat that was too thick or too hot. Check the surface under good light before you decide on a fix.
What Causes Dimples in Epoxy
Dimples usually form when something disturbs the surface before it sets. Repaint Now explains that the mixing reaction generates heat, which expands trapped air bubbles so they rise and pop, leaving a dimple. ArtResin lists three main causes: temperature swings, micro dust particles, and over torching.
Resin Obsession adds several other triggers. The resin may be a casting formula that mixes too thin to self-level, the coat may be too shallow, or oily residue may be repelling the resin. Working the resin right as pot time runs out can also leave dimples that will not level out before the cure completes.
Bubbles and pinholes
Bubbles are the most common culprit. They come from aggressive mixing, air escaping from porous wood or concrete, or air trapped around embedded objects. Repaint Now also lists humidity, old epoxy, and pouring too quickly as reasons you may end up with extra bubbles.
Contamination and craters
Dust that lands on wet resin leaves a crater once it is pulled or disturbed. Oil from hands, silicone spray, wax, and tape adhesive can make the resin pull away from a spot. TotalBoat calls this a fish eye, and it appears as a round pocked spot where the coat will not bond.
Orange peel and waves
Wavy, textured surfaces often come from an uneven base, a temperature swing during the cure, or a layer that was poured too thick and got too hot. TotalBoat also links dust and pouring too little epoxy to flood the surface with low spots.
How to Fix Dimples in Epoxy
The right fix depends on depth. Repaint Now says dimples under 1/16 inch can be fixed with a newer flood coat of doming resin, since doming resins self-level up to 1/8 inch. Clean the surface thoroughly first, then mix and pour a fresh coat that fully covers the area.
Deeper dimples take more work. Repaint Now’s dimple repair article describes dimples about 1/8 inch deep or more as harder to fix, and recommends the steps below.
- Remove debris. Scrape loose material out of the divot with a putty knife.
- Sand flush. Sand the edges until the divot is level with the surrounding surface, sanding evenly so you do not create new low spots.
- Clean the dust. Wipe the area with a clean cloth. TotalBoat recommends denatured alcohol or acetone before a recoat.
- Sand the full surface. TotalBoat suggests 120- to 180-grit for ripples and drips, 220-grit for scratches, and 320-grit before recoating so the new coat can bond.
- Mix a fresh batch. Measure carefully, then mix slowly and scrape the sides and bottom of the cup.
- Overfill slightly. Spread the resin into the divot and leave it a little high.
- Let it cure and sand lightly. Repaint Now suggests at least 24 hours before a light final sanding.
For a fish eye or craters that will not stay filled, TotalBoat table top epoxy guide advises sanding the area, wiping it with acetone, and pouring enough epoxy to flood the surface. A thin coat is more likely to pull away again.
Dimples in Resin vs. Epoxy: Key Differences
Many people use resin and epoxy interchangeably, but the product type affects how dimples behave. Epoxy resin is the broad family of two-part systems. Within it, casting resin is thin and built for deep pours, while doming resin is thicker and built to self-level across a surface.
Resin Obsession states that casting resins mix thin and will not self-level, so a doming resin should be used for coating a surface. Doming resins self-level to about one-eighth inch, so a pour deeper than that needs a dam. The table below sums up the main differences.
| Factor | Casting resin | Doming or coating resin |
|---|---|---|
| Flow | Thin, pours deep | Thicker, stays on the surface |
| Self-leveling | Does not level a coat | Self-levels to about 1/8 inch |
| Dimple risk on a coat | Higher | Lower when mixed enough |
| Best use | Molds and deep pours | Tabletops and surface coats |
Check the product data sheet before you start. The manufacturer lists the maximum pour depth and the self-leveling range for each product.

How to Prevent Dimples During Mixing and Pouring
Prevention is faster than repair. Start with clean surfaces and accurate measurements. Resin Shop Australia recommends mixing for at least 3-5 minutes, scraping the sides and bottom, and using a double-cup method to catch unmixed material.
Measure by the ratio on the label. TotalBoat specifies 1:1 by volume for many tabletop systems, and 1.2:1 by weight for its TableTop product. Pour from the second cup rather than scraping the first one onto the project, since that can deposit unmixed epoxy on the surface.
- Wipe the surface with isopropyl alcohol or acetone before each coat.
- Remove wax, oily residue, and tape adhesive before coating.
- Pour only enough to flood the surface, then spread it evenly.
- Pour before pot time runs low, and stop working the resin once it starts to thicken.
Curing Conditions That Lead to Surface Dimples
Temperature and humidity affect how smoothly the surface sets. ArtResin advises keeping the room stable at 75-85°F (24-30°C) for the first 24 hours, since fluctuations during that window can cause dimples. Resin Shop Australia recommends a controlled space ideally between 18-25°C, and advises against pouring in humid or wet weather.
TotalBoat recommends keeping relative humidity no higher than 60% during work and cure, and curing between 65-80°F. Check your product’s data sheet for its own range, since the numbers differ between brands. Store resin and hardener sealed, and let materials reach room temperature before you use them.
Pour thickness matters too. Resin Shop Australia says to follow the manufacturer’s maximum, such as 10-20 mm per layer, and to pour deeper projects in layers. TotalBoat suggests keeping a fresh flood coat no thicker than 1/4 inch so it can self-level.
Tip: Mix a little more resin than the calculator says, so you are not forced to stretch the last few ounces across the surface.
Safety Tips When Sanding and Recoating
Sanding cured epoxy creates fine dust, and wet resin can irritate skin. Wear nitrile gloves when mixing and when you touch prepped surfaces. Work in a ventilated area, and wear a dust mask or respirator if the sanding is dusty. Read the product’s safety data sheet for specific guidance.
Safety: Use nitrile gloves, keep the space ventilated, and check the SDS for the solvent you use to clean the surface. Never let children or pets near uncured resin or sanding dust.
Use hand sanding or a random orbital sander with a dust collection system. Vacuum the surface before wiping it down. Avoid open flames near solvents such as acetone or denatured alcohol.
For more fixes on cured surfaces, see how to remove epoxy if a section needs to come out completely. If sticky residue gets on your hands during cleanup, how to get resin off hands covers safe removal.
Troubleshooting Checklist and When to Start Over
Use this checklist after each pour. Match the defect to the likely cause, then choose the fix. You can also find related problem-solving articles in our Troubleshooting & Fixes section.
- Tiny pinholes: Check mixing time and bubbles. Sand lightly and recoat.
- Round craters with a raised edge: Check for contamination or dust. Clean and recoat.
- Shallow dips under 1/16 inch: Pour a fresh doming coat.
- Deep divots near 1/8 inch or more: Sand flush, etch, fill, and sand again.
- Wavy texture: Check the table level, room temperature, and layer thickness.
Start over when the surface is tacky, not just dimpled, or when the defect runs through the full thickness. Soft or sticky epoxy will not firm up under a new coat, so scrape it off and clean the area before you pour again. Mixed up with a wrong ratio, the cure may also fail, so measure carefully the second time.
Frequently Asked Questions
What causes dimples in epoxy resin?
Trapped air bubbles that rise and pop are the most common cause, since the mixing heat expands them. Dust, oily residue, temperature swings, and working the resin too close to the end of pot time can also leave dimples.
How do I fix dimples in epoxy resin after it has cured?
For dimples under 1/16 inch, a fresh flood coat of doming resin is usually enough after cleaning the surface. For deeper divots, scrape out debris, sand flush, clean, fill with freshly mixed resin, and let it cure before a light sanding.
Can I fix dimples in epoxy with a heat gun or hairdryer?
A heat gun or hairdryer can help smooth small dimples while the epoxy is still wet, as long as you hold it back so you do not melt or scorch the surface. Once the epoxy has cured, heat will not fix the dimple and you will need to sand and recoat.
What temperature should epoxy be cured at to avoid dimples?
ArtResin advises a stable 75-85°F (24-30°C) during the first 24 hours of cure. TotalBoat cites 65-80°F for its tabletop products, so check your product’s data sheet and keep the room steady.

Dimples in epoxy are usually fixable once you identify the cause. Start with a clean surface, measure carefully, and keep the temperature steady during cure. A good fix is often a sanded, recoated surface, and a careful next pour will help you avoid the problem altogether.
More in Troubleshooting & Fixes
How to Fix Scratches in Epoxy Tables Without Redoing the Whole TopUpdated Nov 26, 2026
How to Remove Amine Blush From Epoxy Without Starting OverUpdated Nov 26, 2026
What Will Remove Epoxy from Wood, Metal, Skin and Hair SafelyUpdated Nov 26, 2026
Paint and Epoxy Remover: Which Type Strips Cured Epoxy and Paint SafelyUpdated Nov 26, 2026
Why Is My Epoxy Bumpy? Causes and Fixes for a Smooth FinishUpdated Nov 26, 2026