Envirotex Lite pour on instructions start with measuring equal amounts of Part A resin and Part B hardener, then mixing thoroughly in two separate cups. Pour within about 25 minutes of mixing at 70°F, since working time gets shorter in warmer rooms. Pop bubbles with a torch held 3 to 4 inches above the surface, and let the coat cure for at least 48 to 72 hours in a dust-free space. Keep the room between 70°F and 80°F and humidity below 50% for the best results.
Envirotex Lite is a two-part pour-on coating that levels into a glossy, clear surface. The steps look simple, but small mistakes such as uneven measuring or skipping the second mix can leave soft or sticky spots. This guide walks through each stage in order, so you can prepare your piece, mix correctly, pour cleanly, and troubleshoot problems if they appear.
What Is Envirotex Lite Pour-On?
Envirotex Lite is a water-clear, two-part epoxy coating sold for flooding a flat surface with a high-gloss finish. The manufacturer describes it as a 1:1 system, so the resin and hardener must be measured in equal volumes. According to the product listing from the manufacturer’s distributor, it is used on artwork, table tops, and crafts.
The coating is designed to self-level, which means it spreads out on its own when the surface is level. One coat is often enough for a deep finish, although two or more coats can be applied if needed. The instructions are printed inside the product box and are also posted on the ETI website.
Envirotex Lite is not the same as a deep pour casting resin. It is meant for thin flood coats over a surface, not thick castings. If you plan a thick block, compare products before you start by reading deep pour vs table top epoxy.
What You Need Before You Start
Gather every supply before you open the bottles, because the mix becomes workable for only a short time. A clean, dry, dust-free room and a level work surface matter as much as the coating itself. Plan on a few disposable containers and a straight-edged stir stick. How to Pour Epoxy Resin in Molds explains a closely connected part of this problem.

| Item | Why you need it |
|---|---|
| Envirotex Lite kit (Part A resin and Part B hardener) | The two parts must be measured in exactly equal amounts |
| Straight-sided, flat-bottom mixing cups | Two cups are used so the mix can be re-stirred without unmixed material |
| Mixing container at least 50% larger than the mix | Leaves room to scrape the sides and bottom while stirring |
| Wood stir sticks with a straight edge | Lets you scrape the bottom and sides of the cup |
| Plastic spatula or stiff card | Helps spread the coating into corners and across edges |
| Disposable cups or small blocks to raise the piece | Lets excess resin drip off the sides without gluing the piece down |
| Wax paper, plastic sheeting, or a catch tray | Protects your work area from drips |
| Nitrile gloves and good ventilation | Keeps resin off your skin and reduces fumes |
| Small propane torch or lighter | Used for popping bubbles on the surface |
Surface Preparation and Sealing
Your surface must be dry, clean, and free of dust, dirt, oil, and grease before any coating goes on. Previously finished surfaces need to be sanded for adhesion and cleaned, and any wax or polish should be removed first. The instructions also say to raise the piece so excess coating can run off the edges.
New or porous wood needs a seal coat. Mix about one quarter of the amount you would use for a flood coat, spread it thinly, and scrape off the excess with cardboard or a plastic spatula. This thin film closes the air passages so bubbles are less likely to rise through the wood. Allow the seal coat to cure for about 5 hours before flood coating.
Check the seal coat for a shiny look. Dull spots mean the wood is not sealed, and a second seal coat is needed. Oak and mahogany are more porous, so a second seal coat is often required on those woods. For large wood slabs, the wood moisture content should be 15% or less, which you can check with a moisture meter.
Glue pictures, prints, or fabric down with clear-drying white glue, not spray adhesive. Apply two coats of white glue over the item, letting each coat dry before the next. Round off sharp table or bar top edges with sandpaper or a 1/4-inch cove bit so the finish builds smoothly.
Mixing and Pouring Correctly
Mixing is where most pour-on problems start, so take your time and measure carefully. Warm the bottles to about 70°F before measuring if they feel cold. Measure Part A and Part B in exact equal volumes, and never guess or empty both bottles into one container.
Sources differ on timing. One guide says to stir for a few minutes, then transfer to a second cup and stir again. Another recommends about 2 full minutes in the first cup and 1 more minute in the second cup. Follow the timing printed in your kit’s instructions, and scrape the sides and bottom throughout.
- Measure equal parts. Pour Part A into a clean measuring cup, then add the same amount of Part B.
- Stir in the first cup. Mix with a straight-edged stick and keep scraping the bottom and sides.
- Transfer to a second cup. Pour the mix into a new cup so any unmixed resin or hardener on the first cup’s walls is left behind.
- Stir again. Mix in the second cup with a new stick until the blend looks clear.
- Pour right away. Start near the edge and work toward the center in a circular pattern.
- Spread the coat. Use a clean stick or spatula only where the coating needs help reaching corners.
- Wipe drips. Clean off drips on the sides with a brush while they form, and avoid spreading the coating too thin.
Work quickly after mixing. The instructions list about 25 minutes of working time at 70°F, with less time in warmer rooms. Do not leave the mix sitting in the cup, because it can heat up and set quickly. Readers working through this often move on to Superclear Table Top Epoxy Instructions.
Removing Bubbles and Keeping Dust Out
Bubbles from mixing usually rise within about 10 to 15 minutes of pouring. Wait for them to surface before you use a torch, so you know where they are. Sweep a small propane torch over the surface, keeping it at least 3 to 4 inches from the coating and moving past the edges so the flame never stops on the wet resin.
Avoid holding the flame in one place, which can scorch the surface. Do not use a hair dryer, because it blows lint from the air onto the wet coating. A plastic drop sheet or a tent of fabric over supports can keep dust off while the coat sets. Even fabric can shed particles, so check it before you cover the piece.
Cure the coating in a dust-free place. Temperatures between 70°F and 80°F are ideal, and warmer rooms cure faster. Do not use a propane heater to warm the room, since burning propane adds moisture to the air. Use a small electric heater instead, and keep room temperatures below 100°F.
Safety: Wear nitrile gloves, work in a ventilated room, and read the product’s safety data sheet before you start. Keep the torch away from flammable items and the table covers around your project.
Curing Time and Final Results
The coating gets glossy early, but it needs much longer to reach full strength. The manufacturer states the coating cures to a glossy finish in about 8 hours at 70°F and reaches full strength in about 48 hours. Other instructions say to allow at least 48 to 72 hours before handling or using the piece.

| Stage | Typical timing from the sources |
|---|---|
| Working time after mixing | About 25 minutes at 70°F, less when warmer |
| Bubbles rise after pouring | Within about 10 to 15 minutes |
| Seal coat on porous wood | About 5 hours before flood coating |
| Glossy surface | About 8 hours at 70°F |
| Full cure and strength | About 48 to 72 hours, longer in cooler rooms |
Coverage depends on the kit size. The manufacturer lists the 16 oz kit at 4 square feet and the 64 oz kit at 16 square feet. Average usage is 4 to 6 ounces per square foot, and the coating will not level correctly if it is spread too thin. Buy enough to cover the top and sides of your project with a little extra.
Troubleshooting Common Problems
Most problems with a sticky or soft finish come from measuring, mixing, or environment. Start by checking whether the parts were measured exactly equal and mixed in two cups. If the mix was right, look at humidity and temperature in the room.
| Symptom | Likely cause | What to do |
|---|---|---|
| Soft or tacky spots | Unequal parts or incomplete mixing | Re-measure, mix in two cups, and recoat once the surface has cured |
| Oily film on the surface | High humidity during the cure | Use a dehumidifier and recoat in a room with humidity below 50% |
| Bubbles that stay trapped | Thick seal coat on wood or flame held too close | Scrape off excess seal coat and sweep the torch from 3 to 4 inches away |
| Dull spots on wood | Wood is not fully sealed | Apply a second seal coat and let it cure |
| Dust or lint in the finish | Air currents or a hair dryer | Cover the piece with a drop sheet and skip the hair dryer |
| Wavy edges after several coats | Wide flat edges built up unevenly | Sand the edge with 120 grit paper, wipe clean, and apply a final coat |
Drips on the bottom edge can be sanded off after the coating hardens. Some crafters apply wide plastic tape to the back edge before coating, then peel it off after the cure. Avoid masking tape for this step. Background on this topic is covered in Instructions for a Resin Skull Mold.
For more background on how these coatings behave, read a practical walkthrough such as the Resin Crafts Blog smoothing tutorial. It describes the equal-parts measurement and the bubble-removal steps in a practical context.
Frequently Asked Questions
How long does Envirotex Lite take to cure before it can be used?
Most instructions say to allow at least 48 to 72 hours for the coating to cure. The manufacturer notes the surface gets glossy in about 8 hours at 70°F, but full strength takes about 48 hours. Cooler rooms need longer.
What is the correct mixing ratio for Envirotex Lite?
Envirotex Lite is a 1:1 system, so Part A and Part B must be measured in exactly equal volumes. Mix in one cup, then transfer to a second cup and mix again. Sources differ on exact stir times, so follow the timing printed in your kit.
How much Envirotex Lite do I need per square foot?
Average usage is 4 to 6 ounces per square foot. The manufacturer’s kit sizes cover 2 square feet for the 8 oz kit and 4 square feet for the 16 oz kit. Measure the top and sides of your project before buying.
Can Envirotex Lite be used outdoors or does it need UV protection?
Instructions for outdoor use say to paint over the coating to protect it from UV rays. Without a UV-resistant topcoat, the clear finish is not meant to sit in direct sun. Check the product’s safety data sheet and manufacturer guidance for your project.
Take your time with the mix, and keep the room clean and within the recommended temperature and humidity range. Once the coat has cured fully, add felt or other protection to the bottom of any piece. For a related primer on resin types, visit Resin Basics & Q&A.
More in Resin Basics & Q&A
What Is Vacuum Degassing for Epoxy Resin and How It Removes Trapped BubblesUpdated Nov 26, 2026
Epoxy Full Cure Time: How Long Before Your Project Is Ready to UseUpdated Nov 26, 2026
Deep Pour vs Table Top Epoxy: Which Fits Your Project Depth and Cure TimeUpdated Nov 26, 2026
High Temperature Epoxy for Metal: How to Pick One That Holds Up to HeatUpdated Nov 26, 2026
Amazing Clear Cast Resin Instructions: Mix, Pour and Cure Without BubblesUpdated Nov 26, 2026
How Long for Deep Pour Epoxy to Cure: Demold and Full-Cure Times ComparedUpdated Nov 26, 2026